How To Prevent Deformation And Cracking Of Die Casting Mold

Feb 15, 2019 Leave a message

In the production and processing of die-casting mold parts, due to the complicated shape and structure, there are obvious differences in the cross-sectional dimensions of each part. Therefore, when heat treatment is performed, the heating and cooling rates of the various parts are also different. This condition can result in distinct thermal stresses, tissue stresses, and phase change volumes in various parts of the part. Causes abnormal expansion or contraction of the part volume, which causes a large deviation in size and shape, and even causes cracking.

The causes of heat treatment deformation and cracking of die-casting molds are various, including the chemical composition of the steel and the original structure, the structural shape and cross-sectional dimensions of the parts, and the heat treatment process. In actual production, deformation is often impossible to completely eliminate, and only to minimize the degree of occurrence, but as long as the appropriate means are taken, the cracking situation can be completely avoided.

1

Preparatory heat treatment

The so-called preliminary heat treatment is relative to the final heat treatment, which is to add a preliminary heat treatment step before the final heat treatment, which step can provide a good mechanical performance or microstructure for the final heat treatment. Common preparatory heat treatment processes include annealing, normalizing, and quenching.

 

Quenching heating method and protection of parts

Quenching and tempering are the processes that are most susceptible to deformation and cracking of parts. For some small die-casting molds, slender cylindrical parts or high-alloy steel mold parts, the direct heating quenching method should be avoided, but it should be preheated to 520 to 580 ° C and then placed in a medium temperature salt bath furnace. Heat to quenching temperature. Practice has proved that the parts using this heating method are significantly smaller than the direct quenching in the electric furnace or the reverberatory furnace, and the cracking condition can be basically avoided.

 

In quenching, if the heating temperature of the austenitic parts is too high, the crystal grains will be coarse, and it will easily cause oxidation and decarburization, which will cause deformation and cracking of the parts. If the temperature is biased, the inner holes will shrink and the pore size will be small. Become smaller. Therefore, the upper limit of the temperature should be selected as much as possible within the range allowed by the heating temperature. For alloy steel, the heating temperature is too high, which will cause the inner hole to expand, and the pore size will become larger. It is better to select the lower limit of the allowable temperature.

In addition, in the quenching and tempering treatment, it is necessary to take measures to effectively protect the parts where the parts are easily deformed and cracked, so that the shape is symmetrical with the cross section, and the internal stress is balanced. This is especially true for parts with complex shapes. Commonly used protection methods include baling, filling, and clogging. 

Cooling method optimization and coolant selection

When the die-casting mold parts are heated, they should not be directly placed in the coolant after being taken out of the furnace, which is likely to cause excessive local temperature difference and cause deformation and cracking. The correct method is to pre-cool the part in the air and then quench it in the coolant. In order to ensure that the cooling speed of each part of the part is uniform, the coolant should be properly rotated after the coolant is placed, and the rotation direction is preferably not fixed. 

The choice of coolant is equally important. For alloy steels, austempering or fractional quenching using a hot bath of potassium nitrate and sodium nitrite is an effective method for reducing deformation, especially for processing die-casting molds with complex shapes and precise dimensional requirements. Some porous mold parts have the characteristics of cooling and shrinking in oil, cooling and expanding in nitrate, and rational use of two different media can also reduce the deformation of parts caused by quenching.